Comparative Optimization and Electrochemical Assessment of Hydroxyapatite–Chitosan Composite Coatings on AISI 316L Stainless Steel Deposited by DC and Pulsed-DC Electrophoretic Deposition

Document Type : Original Article

Authors

1 Institute of Sustainable Energy (ISE), University Tenaga Nasional (UNITEN),Malaysia

2 Institute of Sustainable Energy (ISE), University Tenaga Nasional (UNITEN), Malaysia

3 College of Production Engineering and Metallurgy, University of Technology, Iraq

Abstract

The investigation compares microstructural, adhesion-screening, and electrochemical responses of hydroxyapatite–chitosan composite coatings deposited on AISI 316L stainless steel using DC and pulsed DC electrophoretic deposition. A Taguchi L9 design evaluated voltage, deposition duration, nominal HA loading and prepared-substrate roughness. The greatest observed DC thickness was 23.25 µm (run 9: 60 V, 6 min, nominal HA level 3, Ra 0.05 µm); a separately reported confirmation value was 23.45 µm, although the confirmation settings require reconciliation with the laboratory record. From one exposed 10 × 10 mm face (1.00 cm²), the corrosion current densities were 1.8650 × 10⁻⁵, 6.1900 × 10⁻⁷ and 1.1110 × 10⁻⁷ A/cm² for bare 316L, PDC–HA–chitosan and DC–HA–chitosan, respectively. The latter represents a 99.40% reduction compared with the uncoated control. ASTM G102-type uniform penetration rates calculated using assumed 316L equivalent weight and density are estimates rather than independently measured material-loss rates. The coatings are promising for corrosion mitigation; biological compatibility, clinical durability and unequivocal freedom from pitting are not established by the available measurements.

Thickness and morphology were evaluated using a Taguchi L9 design, and cross-cut observations and electrochemical polarization were compared. The maximum thickness observed in the DC L9 series was 23.25 µm. After normalizing corrosion currents to the measured exposed area of 1.00 cm², DC deposition gave the lowest i_corr (1.1110 × 10⁻⁷ A/cm²), representing a 99.40% reduction versus uncoated steel. A uniform-penetration estimate using assumed 316L alloy properties gave 0.001158 mm/year for DC, compared with 0.194391 mm/year for uncoated steel.

Keywords

Main Subjects